If I leave an uncured resin print in an IPA cleaning tank for too long (For example, if I forget to take it out and leave it in over night) will this damage the print?
I'm using Elegoo gray.
If I leave an uncured resin print in an IPA cleaning tank for too long (For example, if I forget to take it out and leave it in over night) will this damage the print?
I'm using Elegoo gray.
From experience (using eSun water washable grey). I had a print with a thin wall (~0.5mm) that I left in 99.8% IPA over night (<24 hours). The next morning, the thin wall had cracked, almost like it had been pushed in the centre. The rest of the print was intact (walls ~1.5mm)
I suspect it had shrunk and the thin wall could not handle this. This resin appears to have more shrinkage compared to other resins I have used.
So, yes, it could, but I suspect it may depend on the resin and print.
EN Parts start to get tacky when the resin concentration is 5-10% in the IPA tank. It is advisable to shake the pieces for several seconds. In this way the solvent goes well in all the interstices. Then let the object soak for a few more minutes. We can repeat the action a second time before leaving a longer drying.
FR Les pièces commencent à devenir poisseuses lorsque la concentration en résine est à 5-10 % dans le bac à IPA. Il est conseillée de d'agitais plusieurs secondes la piéces. De cette manière le solvant va bien dans tous les interstices. On laisse ensuite tremper l’objet encore quelques minutes. On peut refaire l'action une deuxième fois avant de laisser un séchages plus long.